1)crack[英][kr?k][美][kr?k]炸裂
1.Research on cracking reasons of black tailings devitrified glass;黑色尾砂微晶玻璃炸裂原因的研究
2.The annealing principle of float glass was described ,enumerated and analyzed the common issues,such as crack and warp,presented some practical steps to avoid above issues.介紹了浮法玻璃生產中退火的原理,列舉并分析了在退火過程中常見的各種炸裂和翹曲的問題,提出了在實際操作中的具體處理辦法。
3.The crack reasons of curved tempered glass have been discussed for improving the rate of finished products of curved tempered glass.為了提高鋼化玻璃的成品率,對炸裂這一影響彎鋼化玻璃成品率的主要因素進行了探討,指出玻璃結構、 結石、鋼化工藝(加熱、壓彎、冷卻)等是影響彎鋼化玻璃成品率的主要因素。
英文短句/例句
1.Double charge will rive a connon.加倍填藥,炸裂炮膛。
2.An Analysis of Die Breakage Cause in WEDM凹模在線切割過程中炸裂原因的分析
3.The research of dynamic propagation of crack is prevalent in explosion mechanics.爆炸裂紋的動態擴展問題是爆炸力學研究的熱點。
4.Do not pour hot water into the glass or it will crack.不要往玻璃杯里倒熱水,否則它會炸裂的。
5.Study on the breaking trace of window glass cooled with water at high temperature in fire scene火災現場中高溫窗玻璃遇水炸裂痕跡研究
6.Expansion Mechanism and Numerical Simulation of the Explosion Crack in an Infinite Ice Medium無限冰介質中爆炸裂紋擴展機理與數值模擬
7.Boom!The dynamite sent the rocks flying.炸藥轟隆一聲,山石崩裂。
8.A sudden rupture or bursting, as of an automobile tire.爆裂突然的爆炸,如汽車輪胎的爆炸
9.Study of Flooding Mechanism for Fractures after Explosive Fracturing爆炸壓裂后儲層裂縫的滲流機理研究
10.The loud, sharp sound made as a result of either of these actions.爆炸聲,爆裂聲因爆炸或爆裂而產生的高而尖的聲音
11.To come open or fly apart suddenly or violently, especially from internal pressure.爆裂,炸破突然或劇烈的開裂或炸開,尤指由內部壓力而引起的
12.But you don't fry them too long or they break."但不要炸得時間過長否則會破裂。
13.Burst or explode with a loud noise在一聲巨響中爆裂或爆炸
14.go bang ;burst or explode with a loud noise在一聲巨響中爆裂或爆炸.
15.the act of exploding or bursting something.使某物爆裂或爆炸的動作。
16.The hole made by such a rupture.爆裂口這種爆炸形成的洞
17.a canister that is dropped from a plane and that opens to release a cluster of fragmentation bombs over a wide area.從飛機上投下的打開時能夠釋放一串分裂炸彈的炸彈。
18.Excessive detonation has caused the porcelin on this plug to break away.過分的爆炸會引起火花塞上的陶瓷頭的破裂。
相關短句/例句
mold explosion管模炸裂
1.Pipe mold explosion not only seriously influence the ductile cast iron pipe production, but also largely increase the production cost; In addition it is related to operation and maintenance including internal quality,so proper operation and maintenance is the key to resolve mold explosion.管模炸裂不僅嚴重地影響生產,而且極大地增加生產成本。
3)explosive fracturing爆炸壓裂
1.Described are explosive fracturing, explosive cutting, well cleaning, perforating tubing, workover, casing repair, etc.本文通過分析美國《石油文摘》、中國《石油科技期刊庫》檢索到的二十余篇參考文獻 ,介紹石油工程領域完井與修井的爆炸技術 ,有爆炸壓裂、爆炸切割、爆炸松扣、射孔彈、清潔油井、爆炸修套等技術 ,為有關研究提供參考資
2.The explosive fracturing was tested in house in order to solve problem of formation compact caused by smash area around the wellbore resulting from explosive fracturing.針對爆炸壓裂容易在井壁周圍造成粉碎區、形成致密壓實帶的問題,進行了室內爆炸壓裂模擬試驗。
4)glass rupture玻璃炸裂
5)thermal breakage熱炸裂
1.Study on the mechanism of thermal breakage trace of window glass in fire;火災中窗玻璃熱炸裂痕跡形成機理的研究
6)Glassy shell crack玻殼炸裂