1)VBM垂直布里奇曼法
1.PbI_2 single crystal with three different colors were prepared using Vertical Bridgman Method(VBM).以高純Pb和I2單質為原料,采用兩溫區氣相輸運法(TVM)成功合成出單相PbI2多晶原料,并以此為原料,用垂直布里奇曼法(VBM)生長了3種不同顏色的PbI2單晶體。
2.With the presynthesized polycrystals,the integral and gray-black ZnGeP2 single crystals with size of Φ15 mm×25 mm were obtained by modified Vertical Bridgman Method(VBM).以此為原料,采用改進的垂直布里奇曼法(VBM)生長出尺寸為Φ15 mm×25 mm的ZnGeP2單晶體,呈黑灰色,外觀完整、無裂紋。
英文短句/例句
1.Study on Copper Single Crystal Grown by Vertical Bridgman Method垂直布里奇曼法生長銅單晶體的研究
2.Evolution of Solid-liquid Interface of CdZnTe Crystal Growth by Vertical Bridgman Method碲鋅鎘垂直布里奇曼法晶體生長過程固液界面的演化
3.Analysis of Te precipitates in Cd_(0.8) Mn_(0.2) Te single crystal growing by vertical Bridgman method垂直布里奇曼法生長的Cd_(0.8)Mn_(0.2)Te單晶體中Te沉淀相分析
4.d Bridgeman equation比特和布里奇曼方程
5.The Landscape Park of England:From Bridgeman to Brown (Part Two)英國自然風致園——從布里奇曼到布朗(下)
6.The Landscape Park of England:From Bridgman to Brown (part one)英國自然風致園——從布里奇曼到布朗(上)
7.An analysis for the growth process of PbI2 single crystal by bridgman method has been made.本文分析了用布里奇曼法生長碘化鉛單晶體的結晶過程。
8.Some of them are of a more gentle nature, hanging down from the precipices like a sheet of water, shimmering and wavering as if engaging in graceful dancing.有的瀑布懸掛崖前,如珠簾垂落,輕柔曼舞,蔚為奇觀;
9.Besides Manhattan, it has four other boroughs: Brooklyn, Bronx, Richmond, and Queen's.紐約市分為五個行政區:曼哈頓、布魯克林、布朗克斯、里奇蒙德和昆斯。
10.Research of Association Rules Mining Based on Vertical Data基于數據垂直分布的關聯規則挖掘算法研究
11.Wayne Bridge has gone on loan to Fulham for the remainder of the season.韋恩.布里奇租借至富勒姆直到這個賽季結束.
12.normal force法向[正交、垂直]力
13.Riser cables-Sectional specification垂直布線電纜分規范
14.The tablecloth trails on the floor.臺布一直垂到地板上。
15.vertical zonation of land use土地利用的垂直分布
16.test method for flammability of textiles:vertical method織物燃燒試驗法:垂直法
17.Gabriel Heinze could make a shock return to the United first-team for the Good Friday visit of Sunderland.加布里埃爾-海因策可能會在周五曼聯客場挑戰桑德蘭的比賽中令人驚奇的復出。
18.An Algorithm for Feature Selection and Rule Extraction in Vertically Partitioned Environment;一種垂直分布環境下的特征選擇及規則提取算法
相關短句/例句
vertical bridgman method垂直布里奇曼法
1.The high-quality copper single crystals have been successfully grown by the vertical Bridgman method(VBM),using a self-made growth furnace which is heated with four molybdenum disilicide rods.本文采用自制的硅鉬棒單晶生長爐和特制的鍍碳石英生長坩堝,采用垂直布里奇曼法在30℃/cm的溫度梯度下,以10 mm/d的下降速度生長出較高質量的銅單晶體。
3)Cd compensated vertical bridgman methodCd補償垂直布里奇曼法
1.Growth of Cd_(0.9)Zn_(0.1)Te crystals by Cd compensated vertical bridgman method;Cd補償垂直布里奇曼法生長Cd_(0.9)Zn_(0.1)Te晶體
4)Seeded vertical Bridgman method籽晶垂直布里奇曼法
5)Vertical Bridgman (VB) method垂直布里奇曼(VB)法
1.2 Te single crystal was successfully grown by using Vertical Bridgman (VB) method in our laboratory.本實驗采用垂直布里奇曼(VB)法成功地生長出Cd0。
6)MVBM改進垂直布里奇曼法
1.An integral ZnGeP2 single crystal with size of Φ20mm×30mm was obtained by Modi-fied Vertical Bridgman Method (MVBM).用改進垂直布里奇曼法(MVBM)生長出尺寸為Φ20mm×30mm的ZnGeP2單晶體。
延伸閱讀
班布里奇氏反射
[英文]:Bainbridge reflex[解釋]:因心跳加速引起體靜脈壓力升高或右心房擴張。