1)near-stoichiometric近化學計量比
1.Numerical Simulation on Mode Field Distribution in Near-stoichiometric Ti: LiNbO_3 Strip Waveguide Fabricated by VTE Technique;VTE技術制備的近化學計量比Ti:LiNbO_3條形波導模場分布的數值仿真
2.An magnesium(MgO)-doped near-stoichiometric lithium niobate crystal(MgO:SLN)of 40 mm in diameter and 60 mm in length was grown by an improved Czochralski technique from a 58.5]熔體中生長了φ40mm×60mm的摻鎂近化學計量比鈮酸鋰(LiNbO3)晶體。
3.Domain structure of the near-stoichiometric LiNbO_3 crystal grown by double-crucible pulling method and cut along its each direction is analyzed in this paper.本文對采用雙坩堝提拉法生長的近化學計量比LiNbO3 晶體沿其各向切塊腐蝕后通過直接觀察和在金相顯微鏡下觀察,對其各個面的疇結構進行了分析。
英文短句/例句
1.Photorefractive property of near-stoichiometric Fe:LiTaO_3 crystal近化學計量比Fe:LiTaO_3晶體的光折變性能
2.Domain structure moving characterization of near-stoichiometric lithium tantalate近化學計量比LiTaO_3反轉疇運動特性研究
3.Growth of Near Stoichiometric Mg∶Fe∶LiNbO_3 Crystals and Their Optical Performance近化學計量比Mg∶Fe∶LiNbO_3晶體生長及其光學性能
4.Growth and Properties of Zn,Co Co-doped Near-stoichiometric LiNbO_3 CrystalZn,Co雙摻雜近化學計量比LiNbO_3晶體的生長及性能
5.Fabrication and Optical Characterization of Ti-indiffused Near-stoichiometric LiNbO_3 Waveguides鈦擴散近化學計量比鈮酸鋰光波導的制作和光學表征
6.Optical Properties of Co-doped Stoichiometric Lithium Niobate雙摻雜近化學計量比鈮酸鋰晶體的全息光學特性研究
7.Dynamic Simulation for Li-Ti Indiffusion Simultaneous: Fabrication of Near-stoichiometric Ti: LiNbO_3 Optical Waveguide;鋰—鈦同時內擴散制備近化學計量比Ti:LiNbO_3光波導的動態模擬
8.Numerical Simulation on Mode Field Distribution in Near-stoichiometric Ti: LiNbO_3 Strip Waveguide Fabricated by VTE Technique;VTE技術制備的近化學計量比Ti:LiNbO_3條形波導模場分布的數值仿真
9.Growth, Properties and Potential Application of Series LiNbO_3 Crystals同成分、近化學計量比鈮酸鋰晶體生長、性質及應用探索
10.Study on the Growth and Properties of Stoichiometric Lithium Niobate Doped with Cu銅摻雜近化學計量比鈮酸鋰晶體的生長及其性能的研究
11.The Growtgh of Near-Stoichiometric LiNbO_3 and Nd~(3+) Doped LiNbO_3 Crystals Using Bridgman Method近化學計量比及摻Nd~(3+)鈮酸鋰晶體的下降法生長研究
12.Charge Transport Process in Mn-doped Stoichiometric Lithium Niobate錳摻雜近化學計量比鈮酸鋰晶體的電荷輸運過程
13.Study on growth and photorefractive of near-stoichiometric LiNbO_3 crystal of double-doped with Cu and Fe銅鐵雙摻近化學計量比鈮酸鋰晶體生長及其光折變性能研究
14.The relation of light intensity and the domain switching voltage of the near-stoichiometric Mg-doped lithium niobate was studied.研究了在可見光誘導條件下的近化學計量比摻鎂鈮酸鋰的反轉電壓與光強之間的關系。
15.Comparison of two chemometrics methods in common use for the glucose concentration using near infrared spectra;血糖近紅外光譜分析中兩種常用化學計量學方法的比較
16.Stucture and Photorefractive Properties of Fe: Stoichimetric Lithium Niobium Crystals;化學計量比Fe: LiNbO_3結構與光折變性能
17.Preparation of Stoichiometric Boron-Carbon Ceramics by Spark Plasma SinteringSPS反應燒結不同化學計量比硼-碳陶瓷
18.Synthesis of Stoichiometric LiNiO_2 by Carbon Element Addition添加碳元素合成化學計量比LiNiO_2
相關短句/例句
near stoichiometric近化學計量比
1.A kind of Mg-doped near stoichiometric LiNbO3 crystal was grown with Czochralski method from a stoichiometric melt with addition of llmol% K20 and lmol% MgO.利用提拉法,從摻入11mol%KzO和1mol%MgO的化學配比LiNbO3熔體中生長了高質量的摻鎂近化學計量比LiNbO3晶體。
2.9% K 2O (in mole) flux in raw materials of LiNbO 3 crystal, Fe doped near stoichiometric LiNbO 3 (SLN∶Fe) crystal were grown by top seeded solution growth (TSSG) method and Fe doped congruent LiNbO 3(CLN∶Fe) were grown by Czochralski method.9%K2 O(摩爾分數 )助熔劑 ,用頂部籽晶 (TSSG)法生長近化學計量比摻鐵鈮酸鋰 (SLN∶Fe) ,以及采用Czochralski法生長同成分摻鐵鈮酸鋰 (CLN∶Fe)。
3)stoichiometric近化學計量比
1.Optical Properties of Co-doped Stoichiometric Lithium Niobate雙摻雜近化學計量比鈮酸鋰晶體的全息光學特性研究
2.However, the composition of LiNbO_3 crystal de- viated from its stoichiometric ratio, the existence of lithium vacancies and antib- it niobium defects, and result in many carrier traps, space charge easily be capt- ured, which led to the disadvantage of crystal response time of long, small coup- ling gain coefficient and anti-light-induced scattering ability of low.盡管近化學計量比的晶體比同成份配比的本征缺陷少,但仍然存在摩爾分數為1%的反位鈮和摩爾分數為4%的鋰空位以及大量的極化子、雙極化子、氫離子、局域鈦鐵礦等缺陷結構。
4)near-stoichiometric LiNbO3 single crystal近化學計量比LiNbO3
5)nearly-stoichiometric LiTaO3近化學計量比鉭酸鋰
1.Ultraviolet laser-induced ferroelectric domain inversion in nearly-stoichiometric LiTaO3 was investigated.對紫外激光誘導近化學計量比鉭酸鋰晶體鐵電疇反轉進行了實驗研究。
6)Stoichiometric LiNbO3近化學計量比鈮酸鋰