1)AgGaS2硫鎵銀
1.The thermal analysis kinetics of AgGaS2 crystal was studied by differential scanning calorimetry(DSC).本文利用差示掃描量熱法對硫鎵銀進行了熱分析動力學研究。
2.Silver gallium sulfide(AgGaS2) is a I -III-VI2 ternary compound semiconductor that Crystallizes in chalcopyrite structure (point group D2d-42m).硫鎵銀(AgGaS_2)晶體是典型的Ⅰ-Ⅲ-Ⅵ_2族化合物半導體,屬黃銅礦結構(點群D_(2d)-42m)。
3.A new etchant which is able to selectively etch(112)faces of AgGaS2 crystals at room temperature was reported.本文報道了一種能在室溫下對硫鎵銀晶體(112)面進行擇優腐蝕的新腐蝕液配方,采用新腐蝕液對改進的Bridgman法生長的AgGaS2晶體進行腐蝕,用掃描電鏡對蝕坑進行了觀察,得到了清晰的(112)面蝕坑形貌,形狀為三角錐形。
英文短句/例句
1.Growth and Characterization of AgGaS_2 Single Crystals;硫鎵銀(AgGaS_2)單晶體生長及其性能表征
2.Study on Polycrystal Synthesis and Single Crystal Growth of AgGaS_2;硫鎵銀(AgGaS_2)多晶合成與單晶生長研究
3.Study on Etch Pits Morphology on the(112)Face of AgGaS_2 Crystals硫鎵銀晶體(112)面蝕坑形貌研究
4.Study on the AgGaS_2 Crystal Growth by Quartz Ampoule Descending Method石英安瓿下降法生長硫鎵銀晶體的研究
5.Synthesis of isobutyl p-hydroxybenzoate catalyzed by gallium sulfate硫酸鎵催化合成對羥基苯甲酸異丁酯
6.Synthesis of Isoamyl Isobutyrate Catalyzed by Gallium Sulphate硫酸鎵催化合成異丁酸異戊酯的研究
7.Study of the Sulfur Passivation in GaAs Microwave Power Mesfet;砷化鎵微波功率場效應晶體管的硫鈍化研究
8.Solvothermal Syntheses and Coordination Modifying of Gallium and Indium Chalcogenides鎵、銦硫屬化合物溶劑熱合成及配位修飾
9.Preparation of Ag-Ga/PMMA Nano-composite Materials by Ultrasonic;超聲制備納米銀鎵合金/PMMA復合材料的研究
10.Study of In Segregation Phenomena during AgGa(1-x)In_xSe_2 Crystal Growth硒銦鎵銀單晶生長過程中In分凝現象研究
11.Preparation of Cadmium Sulphide Thin Film and Its Application on Copper Indium Gallium Diselenide Thin Film Solar Cells硫化鎘薄膜的制備及其在銅銦鎵硒薄膜太陽電池上的應用
12.Zinc Sulfide Concentrates Oxygen Pressure Leaching Two Counter-current Principle and Comprehensive Recovery of Gallium Germanium Technology硫化鋅精礦兩段逆流氧壓浸出原理及綜合回收鎵鍺工藝研究
13.A mixture of sulphuric acid-thiourea-thioglycollic acid is used as selective solvent for free silver sulphide and sulphuric acid-thiourea-ferric sulphate for free native silver.用硫酸-硫脲-硫代乙醇酸溶液選擇溶解硫化銀;用硫酸-硫脲-硫酸高鐵銨溶液選擇溶解自然銀。
14.PVP-Capped Silver Nanoparticles as Catalyst for Oxidative Coupling of Thiols to Disulfides納米銀催化氧化偶聯硫醇制二硫化物
15.a valuable silver ore consisting of silver sulfide (Ag2S).一種貴重的銀礦,由硫化銀組成,(AgS)。
16.Study on Reduction of Silver with Sodium Sulfite from Silver-containing Liquid Waste亞硫酸鈉從含銀廢液中還原銀的研究
17.galinium arsenideph.1. 砷化鎵
18.Gallium[67Ga] Citrate枸櫞酸鎵[67ga]
相關短句/例句
AgGaS_2硫鎵銀
1.A New Method for Growth of AgGaS_2 Single Crystal;硫鎵銀單晶生長新方法探索
2.Studies of Vessel Explosion Prevention in the Synthesis of AgGaS_2 Polycrystalline;防止硫鎵銀多晶合成中容器爆炸的研究
3.Growth of AgGaS_2 Single Crystals by Descending Crucible Method with a Three-temperature-zone Furnace;三溫區坩堝下降法生長硫鎵銀晶體
3)AgGaS2 crystal硫鎵銀晶體
4)AgGaS2 single crystal硫鎵銀單晶體
5)silver gallium disulphide crystal二硫化鎵銀晶體
6)AgGa1-xInxSe2硒銦鎵銀
延伸閱讀
二硫化鎵銀晶體分子式:AgGaS2 CAS號:性質:周期表第Ⅰ,III,VI族元素化合物半導體。共價鍵結合,有一定的離子鍵成分。正方晶系黃銅礦型結構,晶格常數0.575nm。為直接帶隙半導體,室溫禁帶寬度2.70eV。熔點1040℃。采用化學氣相沉積、定向凝固等方法制備。為可見光發光材料和非線性光學材料。