<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

合茬薄地膜的制作方法

文檔序號:371236閱讀:287來源:國知局
專利名稱:合茬薄地膜的制作方法
技術領域:
本發明涉及一種能夠將農田地面全面覆蓋的薄地膜,尤其是 用于兩覆膜地壟之間的空當地進行合茬覆蓋。
背景技術:
目前,眾所周知薄地膜覆蓋農田的方法是兩邊用土壓,中間 留出有空間,無法覆蓋,造成了一個地下濕墑蒸發帶,達不到農 田地面全膜覆蓋保墑的技術需要。

發明內容
為了克服現有地膜無法全膜覆蓋地面的技術不足,本發明提 供了 一種可以方便的將農田地面全膜覆蓋的新技術。
本發明解決其技術問題所采用的技術方案是在薄膜的兩邊 帶有膠救劑。
本發明的有益效果是,可以解決兩覆膜地壟之間的空當地濕 墑蒸發的弊病。從而實現了農田地面全膜覆蓋的技術要求。


下面結合附圖和實施例對本發明進一步說明。
圖l是本發明的平面構造圖。 圖中l.薄膜,2.膠粘劑,
具體實施例方式
在圖1中,膠粘劑(2 )涂抹在薄膜(1)的兩邊面上。
權利要求
1.一種方便農田地面全膜覆蓋的合茬薄地膜,其特征是將膠粘劑涂抹在薄膜的兩邊面上。
全文摘要
一種能夠將農田地面全面覆蓋的合茬薄地膜。尤其是可以解決兩覆膜地壟之間空當地濕墑蒸發的缺陷,從而實現了農田地面全膜覆蓋的技術要求。
文檔編號A01G13/02GK101675726SQ200810165950
公開日2010年3月24日 申請日期2008年9月21日 優先權日2008年9月21日
發明者劉清海 申請人:劉清海