<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種玫瑰香內衣面料的加工方法與流程

文檔序號:11083259閱讀:1039來源:國知局

本發明涉及服裝面料領域,尤其是一種玫瑰味內衣面料的加工方法。



背景技術:

現有的內衣面料一般只追求舒適性及保暖性,其次更加注重的是美觀性。而沒有對其內衣面料能散發的味道進行研究。



技術實現要素:

本發明的目的是為了解決上述技術的不足而提供一種玫瑰香內衣面料的加工方法,其能散發出玫瑰的清香,穿著時更加舒適。

為了達到上述目的,本發明所設計的一種玫瑰香內衣面料的加工方法,由紗線前處理、面料織造、面料染色及面料后處理構成,其中,紗線前處理過程中將面料100份、水300份、紅玫瑰提取液20份、黃玫瑰提取液10份、紫玫瑰提取液5份及蘆薈液5份,加熱至45-55℃,保溫160-200min后,取出風干,達到織造條件后在進行面料織造,再進行面料染色及面料后處理;即可。

本發明所得到的一種玫瑰香內衣面料的加工方法,其生產的內衣面料具有一定的玫瑰香味,使得穿著者更加舒適。

具體實施方式

下面通過實施例對本發明作進一步的描述。

實施例1:

本實施例描述的一種玫瑰香內衣面料的加工方法,由紗線前處理、面料織造、面料染色及面料后處理構成,其中,紗線前處理過程中將面料100份、水300份、紅玫瑰提取液20份、黃玫瑰提取液10份、紫玫瑰提取液5份及蘆薈液5份,加熱至55℃,保溫160min后,取出風干,達到織造條件后在進行面料織造,再進行面料染色及面料后處理;即可。

實施例2:

本實施例描述的一種玫瑰香內衣面料的加工方法,由紗線前處理、面料織造、面料染色及面料后處理構成,其中,紗線前處理過程中將面料100份、水300份、紅玫瑰提取液20份、黃玫瑰提取液10份、紫玫瑰提取液5份及蘆薈液5份,加熱至45℃,保溫200min后,取出風干,達到織造條件后在進行面料織造,再進行面料染色及面料后處理;即可。