<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種電力牽引繩索的制作方法

文檔序號:1774849閱讀:544來源:國知局
專利名稱:一種電力牽引繩索的制作方法
技術領域:
本實用新型涉及ー種電纜放線過程中,連接于電纜前端做牽弓I線的繩索。
背景技術:
目前,電纜放線過程中,作為牽引線的多為鋼絲繩,鋼絲繩存在幾個缺點①、自身較重,所需拉カ大,牽引動カ消耗的能源多,或者人工拉動,人工消耗大,較重的鋼絲繩在田間作業時,易損壞莊稼、鋼絲繩,易生銹、老化,使用壽命短、強度不夠高。 發明內容本實用新型目的在于提供ー種拉カ大、重量輕、使用壽命長的電力牽引繩索。本實用新型包括超高分子量聚こ烯長絲纖維編織纜,在所述超高分子量聚こ烯長絲纖維編織纜外設置耐磨纖維護套層。本實用新型所述的編織纜,其強度較大,同等直徑的高分子聚こ烯線纜的拉カ大約是普通鋼絲繩的8 10倍;本牽引線纜自身較輕,消耗的拉カ較小,可節省人工,若機械的牽引動力,其消耗的能源較小;自身輕,在田間作業時,不會損壞莊稼;護套層可保護牽引線,避免其在使用過程中摩擦損壞,使用壽命延長。

圖I為本實用新型的一種結構示意圖。圖中,I、超高分子量聚こ烯長絲纖維編織纜,2、耐磨纖維護套層。
具體實施方式
如圖I所示,本電カ牽引繩索,包括超高分子量聚こ烯長絲纖維編織纜,在超高分子量聚こ烯長絲纖維編織纜外設置耐磨纖維護套層。
權利要求1. 一種電カ牽引繩索,其特征在于包括超高分子量聚こ烯長絲纖維編織纜,在所述超高分子量聚こ烯長絲纖維編織纜外設置耐磨纖維護套層。
專利摘要一種電力牽引繩索,涉及一種電纜放線過程中,連接于電纜前端,做牽引線的繩索。包括超高分子量聚乙烯長絲纖維編織纜,在超高分子量聚乙烯長絲纖維編織纜外設置耐磨纖維護套層。本線纜拉力大、重量輕、使用壽命長。
文檔編號D07B1/16GK202644274SQ20122028238
公開日2013年1月2日 申請日期2012年6月15日 優先權日2012年6月15日
發明者謝春紅 申請人:謝春紅