<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

鋁塑復合板波紋瓦的制作方法

文檔序號:1957156閱讀:385來源:國知局
專利名稱:鋁塑復合板波紋瓦的制作方法
技術領域:
本實用新型屬于鋁塑復合板技術領域,涉及一種鉬塑 復合板波紋瓦。
技術背景現有技術的波紋瓦,由石灰、水泥和麻纖維復合而成。 這種結構的波紋瓦,存在防水效果差、易碎、使用壽命短的問題。
發明內容本實用新型的目的是解決現有技術存在防水效果差、 易碎、使用壽命短的技術問題,提供一種鋁塑復合板波紋瓦,以克服 現有技術的不足。
為了實現上述目的,本實用新型鋁塑復合板波紋瓦,它包括聚乙
稀塑料芯材層,芯材層的上、下面層上設有鋁板;所說鋁板上、下面 層和芯材層經熱熔膠熱壓復合成型。
所說玻紋瓦的截面呈園弧形、梯形或其它形狀。
本實用新型結構設計新穎、合理,解決了現有技術存在防水效果 差、易碎、使用壽命短的技術問題。

附圖是本實用新型截面結構示意圖。
具體實施方式
根據附圖,本實用新型它包括聚乙稀塑料芯材層 2,芯材層2的上、下面層1、 3上設有鋁板;鋁板上、下面層1、 3 和芯材層2經熱熔膠熱壓復合成型;玻紋瓦的的截面形狀呈園弧形、 梯形或其它形狀。
權利要求1、一種鋁塑復合板波紋瓦,其特征是它包括聚乙稀塑料芯材層,芯材層的上、下面層上設有鋁板;所說鋁板上、下面層和芯材層經熱熔膠熱壓復合成型。
專利摘要本實用新型公開了一種鋁塑復合板波紋瓦,它包括聚乙烯塑料芯材層,芯材層的上、下面層上設有鋁板;所說鋁板上、下面層和芯材層經熱熔膠熱壓復合成型。本實用新型結構設計新穎、合理,解決了現有技術存在防水效果差、易碎、使用壽命短的技術問題,可廣泛用于房屋和活動板房的屋頂建設。
文檔編號E04D1/02GK201330475SQ20082023267
公開日2009年10月21日 申請日期2008年12月23日 優先權日2008年12月23日
發明者孫存良, 楊玉斌, 杰 陳, 陳立勇 申請人:蔣云忠