<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

透氣人造革的制作方法

文檔序號:2473626閱讀:132來源:國知局
專利名稱:透氣人造革的制作方法
技術領域:
本發明涉及一種人造革。
背景技術:
一般的人造革具有了手感細膩,延展性柔韌性好等一些天然皮革具有的優點,可是在透氣性能方便確實欠佳,對實際使用造成一定的影響。

發明內容
本發明的目的在于克服上述不足,提供一種透氣功能強大的人造革。
本發明的目的是這樣實現的一種透氣人造革,下層為基質層,上層為面層,所述基質層為超細纖維做成的水刺布,所述面層為聚氨酯做成,面層設有許多細孔。與現有技術相比,本發明的有益效果是本發明由于基質層為超細纖維做成的水刺布,面層設有細孔,使得該人造革的透氣性能大大加強。


圖I為本發明的結構示意圖。其中基質層I、面層2、細孔3。
具體實施例方式參見圖1,本發明涉及的一種透氣人造革,下層為基質層1,上層為面層2,所述基質層I為超細纖維做成的水刺布,所述面層2為聚氨酯做成,面層2設有許多細孔3。
權利要求
1.一種透氣人造革,下層為基質層(I),上層為面層(2),其特征在于所述基質層(I)為超細纖維做成的水刺布,所述面層(2)為聚氨酯做成,面層(2)設有許多細孔(3)。
全文摘要
本發明涉及一種透氣人造革,下層為基質層(1),上層為面層(2),其特征在于所述基質層(1)為超細纖維做成的水刺布,所述面層(2)為聚氨酯做成,面層(2)設有許多細孔(3)。本發明由于基質層為超細纖維做成的水刺布,面層設有細孔,使得該人造革的透氣性能大大加強。