<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

油罐車筒身拼板自動焊工藝的制作方法

文檔序號:11878640閱讀:來源:國知局

技術特征:

1.油罐車筒身拼板自動焊工藝,其特征在于:包括以下步驟:

I、正面焊接:對筒身拼板圈彎接合處采取正面焊透至雙面成型;

II、背面焊接:步驟I完成后,翻轉筒身拼板,在焊縫背部余高上進行不填絲自熔焊;

正面焊接的焊接參數:焊接小車行走速度215mm/min,Ih:410A,Il:330A,Ic:325A,U:17.2v,wfs:220cm/min,F:1.3HZ,Fac:54HZ,N:70%,Nac:70%,氣體流量:25L/min;

背面焊接的焊接參數:焊接小車行走速度215mm/min,Ih:310A,Il:240A,Ic:225A,U:16.0v,F:1.3HZ,Fac:54HZ,N:70%,Nac:70%,氣體流量:25L/min。