<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種具有可沖壓性的金屬涂料的制作方法

文檔序號:12164168閱讀:524來源:國知局

本發明涉及金屬涂料領域,尤其涉及一種具有可沖壓性的金屬涂料。



背景技術:

金屬涂料是用在物體表面可以用來保護物體內部不受到腐蝕的一類油漆。它是工業建設中比防腐漆較常用的一類油漆,廣泛應用於航空、船舶、化工、輸油琯道、鋼結搆、橋梁、石油磚井平臺等領域,深受廣大建筑廠商青睞,但是現有的配套性普遍一般。



技術實現要素:

所要解決的技術問題是克服現有技術存在的缺陷,提供一種具有可沖壓性的金屬涂料。

本發明所采用的技術解決方案是一種具有可沖壓性的金屬涂料,主要成分為含水硅酸鹽礦物,其特征在于:還加入了防腐防霉劑15-20份、改性聚氨酯分散劑5-15份,羧甲基纖維素鈉15-20份、硬酯酸鋅5-10份。

與現有技術相比,本發明所具有的有益效果為:本發明通過加入防腐防霉劑、改性聚氨酯分散劑,羧甲基纖維素鈉、硬酯酸鋅,使得該金屬涂料具有很好的效果。

具體實施方式

本發明詳細內容結合實施例加以說明:

實施例1:一種具有可沖壓性的金屬涂料,主要成分為含水硅酸鹽礦物,其特征在于:還加入了防腐防霉劑15-20份、改性聚氨酯分散劑5-15份,羧甲基纖維素鈉15-20份、硬酯酸鋅5-10份。

實施例2:一種具有可沖壓性的金屬涂料,主要成分為含水硅酸鹽礦物,其特征在于:還加入了防腐防霉劑15-20份、改性聚氨酯分散劑5-14份,羧甲基纖維素鈉15-20份、硬酯酸鋅5-10份。