<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種耐腐蝕合金包裝的制作方法

文檔序號:4161662閱讀:137來源:國知局
專利名稱:一種耐腐蝕合金包裝的制作方法
技術領域:
本實用新型屬于化合物技術領域,特別涉及一種耐腐蝕合金包裝。
背景技術:
目前強酸或強堿的包裝一般采用玻璃瓶,由于玻璃具有易碎的特點,導致強酸或強堿外泄,不安全,并且浪費資源。
發明內容針對現有技術存在的不足,本實用新型提供一種耐腐蝕合金包裝。本實用新型的技術方案是這樣實現的:該合金包裝包括基體、鋁鎂合金層和鎳基合金層;其中基體表面噴涂鋁鎂合金層,鋁鎂合金層表面噴涂鎳基合金層。本實用新型的優點是:通過該包裝,能夠耐強酸和強堿,并且不容易破碎,安全環保。

圖1是本實用新型結構示意圖;圖中:1基體、2鋁鎂合金層、3鎳基合金層;
具體實施方式
本實用新型詳細結構結合附圖和具體實施方式
加以說明。如圖1所示,該合金包裝包括基體1、鋁鎂合金層2和鎳基合金層3 ;基體I采用鋁合金,在鋁合金表面用QT—E— 7/h型噴槍將呈微融熔狀態的含鋁40%-50%和鎂20%-30%的粉末噴涂,之后采用QT— E— 7/h型噴槍在鋁鎂合金層2表面,將呈微融熔狀態的含鎳43%-81%的粉末噴涂。
權利要求1.一種耐腐蝕合金包裝,其特征在于:該合金包裝包括基體、鋁鎂合金層和鎳基合金層;其中基體表面噴涂鋁鎂合金層,鋁鎂合金層表面噴涂鎳基合金層。
專利摘要一種耐腐蝕合金包裝,屬于化合物技術領域。該合金包裝包括基體、鋁鎂合金層和鎳基合金層;其中基體表面噴涂鋁鎂合金層,鋁鎂合金層表面噴涂鎳基合金層。本實用新型的優點是通過該包裝,能夠耐強酸和強堿,并且不容易破碎,安全環保。
文檔編號B65D85/84GK202967164SQ20122056572
公開日2013年6月5日 申請日期2012年10月31日 優先權日2012年10月31日
發明者李翠 申請人:沈陽創達技術交易市場有限公司