<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種密封圈的制作方法

文檔序號:1373975閱讀:271來源:國知局
專利名稱:一種密封圈的制作方法
技術領域:
本實用新型涉及高壓鍋上的一種密封圈。
高壓鍋上現有的密封圈,用的時間太短,短則兩、三個月、長則半年就逐漸失去原有的密封效果。不僅增加消費者的負擔,而且造成原料的浪費。
本實用新型向公眾提供一種經久耐用的密封圈。
本實用新型的結構是高壓鍋上的橡膠密封圈1內嵌入一根鋼絲圈2。鋼絲圈2兩端頭不連接,讓鋼絲圈2有一定的彈性與張力。


圖1 鋼絲圈2的示意圖圖2 密封圈剖面結構圖本實用新型能增強高壓鍋的蓋體與鍋體的密封性能,延長密封圈的使用壽命至兩年以上,節約了制造密封圈的材料。
權利要求1.用于高壓鍋上的一種密封圈,包括原有的橡膠密封圈,其特征在于在高壓鍋的橡膠密封圈1內嵌入一根鋼絲圈2。
2.根據權利要求1所述的一種密封圈,其特征在于鋼絲圈2端頭不連接。
專利摘要用于高壓鍋上的一種密封圈,在原有的橡膠密封圈內嵌入一根鋼絲圈。鋼絲圈的端頭不連接。本實用新型能增強高壓鍋的密封性能,延長密封圈的使用壽命,節約制造密封圈的材料。
文檔編號A47J27/08GK2083450SQ9022564
公開日1991年8月28日 申請日期1990年12月3日 優先權日1990年12月3日
發明者黃應林 申請人:黃應林