<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種弧形陶瓷磚的成型模具的制作方法

文檔序號:2019125閱讀:449來源:國知局
專利名稱:一種弧形陶瓷磚的成型模具的制作方法
技術領域:
本實用新型涉及成型模具的構造,特別是用于弧形磚成型的模具。
本實用新型的技術方案為一種弧形陶瓷磚的成型模具,包括有用于放置磚坯的外模具,外模具上形成有內凹的圓柱面,還增加有一內模芯,內模芯具有與內凹圓柱面對應配合的外圓柱面,內模芯可放入外模具內將磚坯夾于中間并施壓。
采用這樣的技術方案,具有明顯的優點1、模具整體構造不復雜,加工效率高;2、成型的弧形陶瓷磚質量保證、弧形精度高、偏差小。
以下結合附圖和實施例對本實用新型作詳細闡述。


圖1是傳統模具的成型示意圖;圖2是本實用新型的結構示意圖;圖3是本實用新型的成型示意圖;圖4是圖3的A-A剖視圖。
權利要求1.一種弧形陶瓷磚的成型模具,包括有用于放置磚坯的外模具,外模具上形成有內凹的圓柱面,其特征在于還增加有一內模芯,內模芯具有與內凹圓柱面對應配合的外圓柱面,內模芯可放入外模具內將磚坯夾于中間并施壓。
專利摘要本實用新型公開了一種弧形陶瓷磚的成型模具,包括有用于放置磚坯的外模具,外模具上形成有內凹的圓柱面,還增加有一內模芯,內模芯具有與內凹圓柱面對應配合的外圓柱面,內模芯可放入外模具內將磚坯夾于中間并施壓,這樣的模具,生產出的弧形磚整體均勻一致,弧度偏差小,且生產效率高、質量好、易于調整,克服了傳統模具變形大、不一致率高等成型的缺陷。
文檔編號B28B7/00GK2487529SQ01233880
公開日2002年4月24日 申請日期2001年8月2日 優先權日2001年8月2日
發明者吳小福, 霍錦煊, 李潤南, 霍錫燦 申請人:霍錦煊, 李潤南, 霍錫燦