<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

鋼制防火門的制作方法

文檔序號:2202573閱讀:279來源:國知局
專利名稱:鋼制防火門的制作方法
技術領域:
本實用新型涉及一種鋼制防火門。
背景技術:
鋼質防火門門扇結構為內外兩張鋼板,中間填充硅酸鋁棉,生產時需將兩張鋼板與硅酸鋁棉通過壓機壓制成型。通常壓機為冷壓機,常溫常壓,其最大缺點是工作時間長,尤其是冬天工作時間更長(要
達到12小時)。
實用新型內容
本實用新型針對上述缺陷,目的在于提供一種具有阻燃性能、且能進行高效生產的鋼制防火門。
本實用新型的技術方案是本實用新型包括兩鋼板,兩張適配的鋼板熱壓復合成長方體門形,兩鋼板中間填充硅酸鋁棉。
本實用新型用熱壓機取代冷壓機膠合門扇大大縮短了工作時間,膠合時間由原來的8小時縮短到現在的0.5小時,提高了生產效率的同時也減少了設備的投入,并且門扇的平整度和整體強度也有所提高,同時在兩鋼板中間填充和兩鋼板復合成一體的硅酸鋁棉,使得本實用新型的門具有良好的阻燃性能。


圖1為本實用新型的結構示意圖
3圖中1為鋼板、2為硅酸鋁棉。
具體實施方式

本實用新型包括兩鋼板l,兩張適配的鋼板1熱壓復合成長方體門形,兩鋼板l中間填充硅酸鋁棉2。
權利要求1、鋼制防火門,其特征在于,兩張適配的鋼板熱壓復合成長方體門形,兩鋼板中間填充硅酸鋁棉。
專利摘要鋼制防火門。包括由兩張適配的鋼板熱壓復合成長方體門形,兩鋼板中間填充硅酸鋁棉。本實用新型用熱壓機取代冷壓機膠合門扇大大縮短了工作時間,膠合時間由原來的8小時縮短到現在的0.5小時,提高了生產效率的同時也減少了設備的投入,并且門扇的平整度和整體強度也有所提高,同時在兩鋼板中間填充和兩鋼板復合成一體的硅酸鋁棉,使得本實用新型的門具有良好的阻燃性能。
文檔編號E06B5/16GK201420489SQ20092004089
公開日2010年3月10日 申請日期2009年4月20日 優先權日2009年4月20日
發明者徐正祥, 時榮州, 趙國平 申請人:江蘇省金鑫安防設備有限公司