<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

固定窗鋁合金外框的制作方法

文檔序號:11091815閱讀:來源:國知局

技術特征:

1.固定窗鋁合金外框,其特征在于,包括:

外框基體,采用鋁合金型材制成,其具有一主板,該主板的底部兩側具有用于連接墻體的腳撐,該主板的頂部一側具有自該側腳撐向上延伸而成的框沿,該框沿的底部內側具有第一卡槽,該主板的頂部另一側具有與第一卡槽相對設置的第二卡槽;

夾緊件,采用鋁合金型材制成,其具有一配合框沿以夾持玻璃的夾持部,該夾持部的底部具有與第一卡槽緊配的第一彎折部,該夾持部的頂部具有與第二卡槽緊配的第二彎折部。

2.根據權利要求1所述的固定窗鋁合金外框,其特征在于:所述的夾持部,其與框沿配合的一側沿其長度方向設有多條平行設置的防滑槽。

3.根據權利要求1所述的固定窗鋁合金外框,其特征在于:所述的第一彎折部,其底面與所述的主板的頂面間隙配合。

4.根據權利要求1所述的固定窗鋁合金外框,其特征在于:所述的第二彎折部是自夾持部的頂部向第二卡槽延伸的斜面。

5.根據權利要求1所述的固定窗鋁合金外框,其特征在于:述的第二彎折部是自夾持部的頂部向第二卡槽延伸的直角彎折面。