<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

低成本抗刮耐磨彩盒彩紙的制作方法

文檔序號:12102536閱讀:433來源:國知局

本實用新型涉及包裝盒技術領域,特別涉及一種低成本抗刮耐磨彩盒彩紙。



背景技術:

我們現在普遍使用的彩盒彩用上油或上膜的表面處理方式,上油產品不防水,上普通BOPP膜產品無感刮傷無法克服,上抗刮膜單價太高,普通產品無法承受此單價,這就需要一種成本低廉的新工藝來解決當前問題,我們此項工藝很好的解決了這一問題。



技術實現要素:

為了克服上述缺陷,本實用新型提供了一種解決上述問題的低成本抗刮耐磨彩盒彩紙。

本實用新型為了解決其技術問題所采用的技術方案是:一種低成本抗刮耐磨彩盒彩紙,包括承印物的紙張、印刷油墨、BOPP啞膜和低氣味UV啞油,在紙張的表面印制印刷油墨后,所述BOPP啞膜位于印刷油墨的上層,所述低氣味UV啞油覆蓋于BOPP啞膜的最外層。

作為本實用新型的進一步改進,所述低氣味UV啞油的亮度控制在10度±3度,其接近BOPP啞膜的亮度。

本實用新型的有益效果是:本實用新型的低成本抗刮耐磨彩盒彩紙,在BOPP啞膜的外側再鋪設一層低氣味UV啞油,能夠代替現有抗刮膜,防止BOPP啞膜被刮傷,且其原料成本低,加工工藝簡便,能夠很好的解決BOPP啞膜被刮傷的問題。

附圖說明

圖1為本實用新型結構示意圖;

圖中標示:1-紙張;2-印刷油墨;3- BOPP啞膜3;4-低氣味UV啞油。

具體實施方式

為了加深對本實用新型的理解,下面將結合實施例和附圖對本實用新型作進一步詳述,該實施例僅用于解釋本實用新型,并不構成對本實用新型保護范圍的限定。

圖1示出了本實用新型一種低成本抗刮耐磨彩盒彩紙的一種實施方式,包括承印物的紙張1、印刷油墨2、BOPP啞膜3和低氣味UV啞油4,在紙張1的表面印制印刷油墨2后,所述BOPP啞膜3位于印刷油墨2的上層,所述低氣味UV啞油4覆蓋于BOPP啞膜3的最外層,所述低氣味UV啞油4的亮度控制在10度±3度,其接近BOPP啞膜3的亮度。