<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

線材入口可移動導槽的制作方法

文檔序號:2990368閱讀:360來源:國知局
專利名稱:線材入口可移動導槽的制作方法
技術領域:
本實用新型涉及一種軋鋼廠用于制作線材入口可移動導槽。
背景技術:
目前軋鋼廠線材飛剪在使用過程中,因飛剪前導槽是固定的,飛剪剪刃只能用中間部分剪切,其他部位不能使用,這樣就需經常更換剪刃,造成極大的浪費,解決這一問題已成為急需。實用新型的內容克服現有技術的不足,設計一種使飛剪剪刃任何部位都可以剪切的線材入口可 移動導槽。線材入口可移動導槽是在飛剪前導槽的前端固定一根絲杠,在導槽尾部下面固定有軸。本實用新型通過移動導槽,使剪刃上任何部位都可以使用,極大提高了剪刃的使用率,使剪刃的使用壽命由原兩天提高到十五天,節省了大量費用。本實用新型同時具有結構簡單、制作方便、造價低、節省成本、安全性高并且可提高工作效率的優點。


圖I為本實用新型正面視圖。
具體實施方式
本實用新型的一個最佳實施例,在飛剪前導槽I的前端焊接上一根絲杠2,可以使導槽橫向移動,在導槽尾部下面焊上軸3,起到穩定導槽的作用,以免在調整絲杠時整個導槽跟著一起移動。
權利要求1.一種線材入口可移動導槽其特征是在飛剪前導槽的前端固定一根絲杠,在導槽尾部下面固定有軸。·
專利摘要一種線材入口可移動導槽是在飛剪前導槽的前端固定一根絲杠,在導槽尾部下面固定有軸。本實用新型通過移動導槽,使剪刃上任何部位都可以使用,極大提高了剪刃的使用率,使剪刃的使用壽命由原兩天提高到十五天,節省了大量費用。本實用新型同時具有結構簡單、制作方便、造價低、節省成本、安全性高并且可提高工作效率的優點。
文檔編號B23D33/02GK202715887SQ201220374019
公開日2013年2月6日 申請日期2012年7月31日 優先權日2012年7月31日
發明者張志明, 溫井峰 申請人:西林鋼鐵集團有限公司