<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種蔬果用的輕質保鮮防腐復合包裝材料的制作方法

文檔序號:11098623閱讀:來源:國知局

技術特征:

1.一種蔬果用的輕質保鮮防腐復合包裝材料,其特征在于:包括以下重量份數的原料:基體樹脂50~100份、新戊二醇二縮水甘油醚3~8份、羥丙基二淀粉磷酸酯5~10份、聚乙烯基吡咯烷酮2~6份、聚丙烯酸鈉1~5份、碳酸鈣1~3份、間苯二酚雙(二苯基)磷酸酯1~3份、羥丙基二淀粉磷酸酯5~10份、羥基硅油1~3份、改性填料0~58份、光穩定劑0.5~2份、抗氧劑0.5~1.5份、抑菌劑0.2~0.8份;

所述基體樹脂為乙烯-1-辛烯共聚物、聚乙烯醇縮丁醛和鉬酚醛樹脂,其質量份比為2~4:1~2:1。

2.根據權利要求1所述的一種蔬果用的輕質保鮮防腐復合包裝材料,其特征在于:所述改性填料為苯乙烯-馬來酸酐共聚物0~30份、氣相二氧化鈦0~20份、羥基磷灰石粉0~8份。

3.根據權利要求1所述的一種蔬果用的輕質保鮮防腐復合包裝材料,其特征在于:所述抑菌劑為3-乙氧基-4-羥基苯甲醛、異噻唑啉酮中的一種或其結合。

4.根據權利要求1所述的一種蔬果用的輕質保鮮防腐復合包裝材料,其特征在于:所述的抗氧劑為雙(2,4-二叔丁基苯基)季戊四醇二亞磷酸酯或2,5-二特丁基對苯二酚。

5.根據權利要求1所述的一種蔬果用的輕質保鮮防腐復合包裝材料,其特征在于:所述光穩定劑為鄰羥基二苯甲酮類、水楊酸酯類或取代丙烯腈類光穩定劑。