<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種蘑菇料的快速堆制方法

文檔序號:385781閱讀:340來源:國知局
專利名稱:一種蘑菇料的快速堆制方法
一種蘑菇料的快速堆制方法
技術領域:
本發明涉及一種蘑菇料的堆制方法。
本發明的目的是堆制一種省時、節能、省力的蘑菇料快速堆制的方法。 本發明是這樣實現的,其特征在于
(1) 先把料堆上邊的草簾揭去,保持原堆的層次,再將暴露在外的料 堆外表覆蓋層翻在原堆的旁邊,并整好堆形,然后將原堆內部的料按順 序一層層地翻開堆蓋在新整好的料堆上面,最后蓋上草簾或塑膜即可。
(2) 按照此法可連續翻堆2—3次即可。
實施例
1. 先把料堆上邊的草簾揭去保持原堆的層次,再將暴露在外的料堆 外表覆蓋后翻在原堆的旁邊,并整好堆形,然后將原堆內部的料按順序 一層層翻開堆蓋在薪整好的料堆上面,最后蓋上草簾或塑膜。
2. 按此法可連續翻堆2次即可
采用本方法堆制蘑菇料能達到發酵均勻,既省工省時省力,且培養料 的質量又好,比常規發酵有著明顯的增產。
權利要求
本發明涉及一種蘑菇料的堆制方法,其特征在于1、先把料堆上邊的草簾揭去保持原堆的層次,再將暴露在外的料堆外表復蓋層翻在原堆的旁邊,整好堆形,然后將原堆內部的料按順序一層層地翻開堆蓋在整好的料堆上面,最后蓋上草簾塑膜。
1、 先把料堆上邊的草簾揭去保持原堆的層次,再將暴露在外的料堆 外表復蓋層翻在原堆的旁邊,整好堆形,然后將原堆內部的料按順序一 層層地翻開堆蓋在整好的料堆上面,最后蓋上草簾塑膜。
2、 根據權利要求l所述按此方法可連續翻堆2-3次。
全文摘要
本發明涉及一種蘑菇料的堆制方法,用本方法堆制的蘑菇料,能達到發酵均勻、省工,省時,且培養料的質量又好,比常規發酵有著明顯的增產。