<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種金屬零件清洗劑的制作方法

文檔序號:12300742閱讀:332來源:國知局

本發明涉及精細化工的技術領域,特別涉及一種金屬零件清洗劑。



背景技術:

金屬零件清洗劑可以被用于金屬零件的清洗,需求量巨大。因此,本行業內需要開發一款清洗效果優異的金屬零件清洗劑。



技術實現要素:

本發明的目的是提供一種金屬零件清洗劑,解決上述現有技術問題中的一個或者多個。

本發明提供一種金屬零件清洗劑,按質量份數計包括以下組分:0.5份的磷酸三鈉、1份的焦磷酸鈉、0.5份的氫氧化鈉、45份的脂肪酸醇聚氧乙烯醚、53份的去離子水。

具體實施方式

下面的實施案例,對本發明進行進一步詳細的說明。

實施案例:

一種金屬零件清洗劑,按質量份數計包括以下組分:0.5份的磷酸三鈉、1份的焦磷酸鈉、0.5份的氫氧化鈉、45份的脂肪酸醇聚氧乙烯醚、53份的去離子水。

本發明實施案例的金屬零件清洗劑,清洗效果明顯,對金屬零件沒有腐蝕作用,且組分的成本低。

以上表述僅為本發明的優選方式,應當指出,對本領域的普通技術人員來說,在不脫離本發明創造構思的前提下,還可以做出若干變形和改進,這些也應視為發明的保護范圍之內。



技術特征:

技術總結
本發明公開一種金屬零件清洗劑,按質量份數計包括以下組分:0.5份的磷酸三鈉、1份的焦磷酸鈉、0.5份的氫氧化鈉、45份的脂肪酸醇聚氧乙烯醚、53份的去離子水。該金屬零件清洗劑,清洗效果明顯,對金屬零件沒有腐蝕作用,且組分的成本低。

技術研發人員:湯健
受保護的技術使用者:湯健
技術研發日:2017.06.16
技術公布日:2017.10.27