<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種制備鋇長石微晶玻璃的方法和系統與流程

文檔序號:11508964閱讀:來源:國知局

技術特征:

技術總結
本發明公開了一種制備鋇長石微晶玻璃的方法和系統。其中,該方法包括如下步驟:步驟1:將BaO、SiO2、Al2O3、B2O3、ZrO2混合均勻,制得混合料;步驟2:將所述混合料加熱至熔融,制得熔融料;步驟3:將KMnO4及Al粉混合均勻后加入到所述熔融料中,并攪拌均勻;步驟4:對步驟3得到的熔融原料進行水萃、燒結以制備鋇長石微晶玻璃;所述Al2O3的用量≤原料總重量的10%。本發明通過加入Al粉及KMnO4兩種物質,部分替代了傳統方法中的鋁源、助熔劑及澄清劑,能有效改善原料的熔融效果。

技術研發人員:馬冬陽;吳道洪;邊妙蓮;孫輝;陳士朝
受保護的技術使用者:江蘇省冶金設計院有限公司
技術研發日:2017.06.28
技術公布日:2017.10.17