<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

擠液輥的制作方法

文檔序號:4758504閱讀:229來源:國知局
專利名稱:擠液輥的制作方法
技術領域:
本實用新型涉及一種銅箔加工設備上使用的擠液輥。
背景技術:
在銅箔加工設備中,尤其是生箔機中,需要將箔上面的硫酸銅溶液或者水 去除掉,通常采用輥壓的方法去掉液體,但是由于常用的輥筒硬度太大,擠液 率太低,使一部分硫酸銅溶液或者水隨著箔流失掉。
實用新型內容
本實用新型的目的是提供一種提高擠液率的生箔用擠液輥。 為實現上述目的,本實用新型采用如下技術方案 一種擠液輥,包括心軸, 心軸外固設有輥筒,輥筒外圈套設有包膠層。 所述包膠層硬度小于邵氏75。 所述包膠層為橡膠層。
本實用新型的有益效果為由于橡膠層有適當的硬度,既不過硬,并且還 具有一定的韌性,套設在輥筒外可以大大提高擠液率。包膠層硬度小于邵氏75
可以起到較好效果,使擠液率達到90%以上。


圖l是本實用新型的結構示意圖。
具體實施方式

由圖1所示的一種擠液輥,包括心軸1,心軸1外焊接有輥筒3,輥筒3 外圈套設有橡膠層2,所述橡膠層2硬度小于邵氏75。
由于橡膠層2有適當的硬度,既不過硬,并且還具有一定的韌性,套設在 輥筒3外可以大大提高擠液率。
權利要求1.一種擠液輥,包括心軸,心軸外固設有輥筒,其特征在于輥筒外圈套設有包膠層。
2. 如權利要求1所述的擠液輥,其特征在于所述包膠層硬度小于邵氏75。
3. 如權利要求1或2所述的擠液輥,其特征在于所述包膠層為橡膠層。
專利摘要本實用新型公開了一種擠液輥,包括心軸,心軸外固設有輥筒,輥筒外圈套設有包膠層。所述包膠層硬度小于邵氏75。所述包膠層為橡膠層。本實用新型的目的是提供一種提高擠液率的生箔用擠液輥。
文檔編號F26B5/14GK201434563SQ200920090230
公開日2010年3月31日 申請日期2009年5月14日 優先權日2009年5月14日
發明者何成群, 李應恩, 薛宏偉, 佩 賈 申請人:靈寶華鑫銅箔有限責任公司