<listing id="vjp15"></listing><menuitem id="vjp15"></menuitem><var id="vjp15"></var><cite id="vjp15"></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><menuitem id="vjp15"></menuitem></video></cite>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<var id="vjp15"><strike id="vjp15"><listing id="vjp15"></listing></strike></var>
<menuitem id="vjp15"><strike id="vjp15"></strike></menuitem>
<cite id="vjp15"></cite>
<var id="vjp15"><strike id="vjp15"></strike></var>
<var id="vjp15"></var>
<var id="vjp15"></var>
<var id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></var>
<menuitem id="vjp15"></menuitem><cite id="vjp15"><video id="vjp15"></video></cite>
<var id="vjp15"></var><cite id="vjp15"><video id="vjp15"><thead id="vjp15"></thead></video></cite>
<var id="vjp15"></var>
<var id="vjp15"></var>
<menuitem id="vjp15"><span id="vjp15"><thead id="vjp15"></thead></span></menuitem>
<cite id="vjp15"><video id="vjp15"></video></cite>
<menuitem id="vjp15"></menuitem>

一種機制砂預應力混凝土制備方法與流程

文檔序號:11080207閱讀:來源:國知局
技術總結
本發明公開了混凝土制備技術領域的一種機制砂預應力混凝土制備方法,所述機制砂預應力混凝土制備方法的具體步驟如下:S1:在拌合機內投放經過級配預先處理的機制砂原料;S2:再投放經過配比的復合摻料;S3:在拌合機內加入水泥;S4:在拌合機內加入外加劑繼續拌和;S5:在澆注混凝土構件前進行綁扎鋼筋,安裝鐵件,支設模板,然后進行澆注;S6:使混凝土構件受拉區的混凝土獲得預壓應力,制備出機制砂預應力混凝土,本發明采用機制砂混入混泥土拌和中,能有效填充骨料間的空隙,使混凝土更加密實,本發明選擇低耗水水泥,可實現混凝土水灰比的降低,有利于形成較高的混凝土強度。

技術研發人員:何盛東;張志友;李銳;劉偉;史偉亞;沈方;胡帥;趙志強;仝曉英
受保護的技術使用者:鄭州航空工業管理學院
文檔號碼:201611151532
技術研發日:2016.12.14
技術公布日:2017.05.10